Improved coating adhesion prevents chipping and provides stable machining |
Micro TiCN coating provides excellent wear resistance |
Hard surface layer - provides advanced wear resistance |
Strong intra coating adhesion - higher adhesion between each layer with improved crystal structure |
Micro TiCN layer - higher coating hardness is possible due to a micro TiCN crystal structure, resulting in increased wear resistance |
CA310 grade for high speed continuous machining and improved tool life through the deposition of a thickened alumina coating layer |
KG chipbreaker - for various cast iron machining applications and chipping resistance is improved in spite of having a positive land |
WSM01 - Applicable on high temperature alloys and austenitic stainless steels |
+/-0.025 mm corner point tolerance |
+/-0.13 mm thickness tolerance |
+/-0.025 mm inscribed circle tolerance |
0.1 to 0.35 mm feed/rev |
9.525 mm cutting edge length |
11 deg rake |